Problem:
Some laminated glass manufacturers may face the problem: when they
edging the laminated glass with Ethylene-vinyl acetate EVA Interlayer
Film, the laminated glass delaminate at edges.
How to avoid this problem?
Contact US:cnc(at)cncnext(dot)com/benext77(at)gmail(dot)com
Reasons and Solutions

1.Do not edging the laminated glass until the laminated glasses have
been cooled for 24 hours after pulled out from the EVA GLASS
LAMINATING OVEN.

2.When edging, SOME heat will be created in the edges, which will do
harm to the EVA FILM adhesion, so please use more water to cool the
heat when edging the laminated glass.
Contact US:cnc(at)cncnext(dot)com/benext77(at)gmail(dot)com
3.Please edging slowly and tenderly.

4.If the EVA FILM interlayer you use is not good quality, then the
adhesive between the EVA Film and glass surface may be weak, then it’s
easy to delaminate when edging.

All rights reserved by:
China (Ethylene-vinyl acetate)EVA Interlayer Film Manufacturer for
Safety Laminated Glass, Smart Glass, Privacy Glass, LED Glass, PV
Solar Encapsulationetc.
cnc2@cncnext.com / www.cncnext.com
eva@evafilms.com / www.evafilms.com
benext77@gmail.com / benext77@hotmail.com